600

High-Temp Steel

600

Ni-Cr alloy, heat & oxidation resistant. (ASTM B637; equiv UNS N06600 / AMS 5540). Nominal values—confirm mill certificate.

Chemical Composition (%)

NI72
CR14
FE6
C0.15
MN1
SI0.5

Mechanical Properties

Tensile(annealed):≥550 MPa;Yield(annealed):≥240 MPa;Elong:≥30%

Chinese Standard

ASTM B637 600

Equivalent Standards

AMS 5540

Equivalent Grades

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.

Applications

镍铬耐热抗氧化。,"Plate

Available Forms

Bar

Uses

Tube"

Heat Treatment

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Precautions

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.