60CrMo3-2

Other

60CrMo3-2 / 1.7240

60CrMo3-2 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.56
SI0.4
MN0.7
P0.025
S0.025
CR0.7
MO0.15

Available Forms

Bar, Plate, Tube, Forging

Uses

Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.85%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.

Heat Treatment

Austenitize at 760–820 °C and quench (oil/water) then temper at 150–400 °C for high hardness; spheroidize anneal (680–720 °C) improves machinability of the as-rolled bar.

Precautions

Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).