616
High-Temp Steel616
Co-W Ni-base alloy. (ASTM B637; equiv UNS N06616). Nominal values—confirm mill certificate.
Chemical Composition (%)
| CR | 20 |
|---|---|
| CO | 10 |
| MO | 7 |
| W | 1.5 |
Mechanical Properties
Tensile:≥900 MPa;Yield:≥600 MPa
Chinese Standard
ASTM B637 616
Applications
钴钨镍基合金。,Bar
Available Forms
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈11.5%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Uses
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Heat Treatment
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.
Precautions
UNS N06616