625

High-Temp Steel

625

Ni-Cr-Mo-Nb alloy, corrosion & high-temp resistant. (ASTM B637; equiv UNS N06625 / AMS 5666 / EN 2.4856 / GB 0Cr20Ni65Mo10Nb4). Nominal values—confirm mill certificate.

Chemical Composition (%)

NI58
CR20
MO8
NB+TA3.15
FE5
C0.1
MN0.5
SI0.5
AL0.4
TI0.4
P0.015
S0.015

Mechanical Properties

Tensile:≥830 MPa;Yield:≥415 MPa;Elong:≥30%;Hardness:≤240 HB

Chinese Standard

ASTM B637 625

Equivalent Standards

AMS 5666

Equivalent Grades

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.

Applications

镍铬钼铌,耐蚀耐高温。,"Bar

Available Forms

Plate

Uses

Wire"

Heat Treatment

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Precautions

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.