65Mn
Alloy Steel65Mn
Spring wire steel. (GB/T 1222; equiv GB 65Mn / DIN 1.0614 / JIS SUP3). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.62 |
|---|---|
| SI | 0.17 |
| MN | 0.9 |
| S | 0.035 |
| P | 0.035 |
Mechanical Properties
Tensile:≥980 MPa;Yield:≥785 MPa;Elong:≥8%;Hardness:≤269 HB
Chinese Standard
T 1222 65Mn
Equivalent Grades
GB 65Mn / DIN 1.0614 / JIS SUP3
Applications
弹簧钢丝钢。,"Bar
Available Forms
Wire"
Uses
High-carbon grade for rails, springs, cutting tools, wear plates and components demanding high hardness and wear resistance after heat treatment. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 760–820 °C and quench (oil/water) then temper at 150–400 °C for high hardness; spheroidize anneal (680–720 °C) improves machinability of the as-rolled bar.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).