706
High-Temp Steel706
Specialty steel grade. ; equiv UNS N09706 / AMS 5607). Nominal values—confirm mill certificate.
Chemical Composition (%)
| NI | 39 |
|---|---|
| CR | 14 |
| NB | 2.5 |
| TI | 1.5 |
Mechanical Properties
Tensile:≥1170 MPa;Yield:≥930 MPa
Chinese Standard
ASTM B637 706
Equivalent Standards
AMS 5607
Equivalent Grades
UNS N09706
Applications
低镍718,加工性好。,"Bar
Available Forms
Forging"
Uses
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Heat Treatment
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Precautions
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.