7075-T42
Aluminum7075 aluminum alloy
7075-T42 supplied by Shanxi Youte Steel (jlhsteel.net).
Chemical Composition (%)
| ZN | 5.1 |
|---|---|
| MG | 2.1 |
| CU | 1.2 |
| CR | 0.18 |
Equivalent Standards
ASTM B209
Equivalent Grades
Aluminum Association / AA 7075
Applications
Aerospace, automotive, construction, packaging, electrical.
Available Forms
Sheet, Plate, Bar, Extrusion, Foil, Tube, Wire
Uses
Aluminium alloy with good strength-to-weight ratio, corrosion resistance and recyclability. Copper (≈1.6%) raises strength and hardness via precipitation hardening. Used in transport, aerospace, packaging, building and electrical applications.
Heat Treatment
Heat-treatable variants solution treated 470–540 °C and aged (T4/T6); non-heat-treatable grades are strain-hardened. Anneal 340–415 °C.
Precautions
Use sharp, high-rake tooling and appropriate coolants; galling/adhesive wear can occur. Titanium reacts with hydrogen and chlorine — keep out of pickling/HCl environments.
Comments 0