909
High-Temp Steel909
Low-expansion superalloy, excellent low-cycle fatigue. (ASTM B637; equiv UNS N19909 / AMS 6544). Nominal values—confirm mill certificate.
Chemical Composition (%)
| NI | 37 |
|---|---|
| CR | 11 |
| CO | 12 |
| MO | 4 |
| NB | 4 |
Mechanical Properties
Tensile:≥1410 MPa;Yield:≥1000 MPa
Chinese Standard
ASTM B637 909
Equivalent Standards
AMS 6544
Applications
低膨胀高温合金,低周疲劳优。,Bar
Available Forms
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈14%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Uses
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Heat Treatment
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.
Precautions
UNS N19909
Comments 0