925(718+)
High-Temp Steel925(718+)
Precipitation-hardened 825 alloy. (ASTM B637; equiv UNS N09925). Nominal values—confirm mill certificate.
Chemical Composition (%)
| NI | 38 |
|---|---|
| CR | 19.5 |
| MO | 2.5 |
| TI | 1.5 |
| AL | 0.1 |
Mechanical Properties
Tensile:≥965 MPa;Yield:≥655 MPa
Chinese Standard
ASTM B637 925(718+)
Applications
沉淀硬化825。,Bar
Available Forms
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Uses
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Heat Treatment
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.
Precautions
UNS N09925
Comments 0