94B17 Normalized & Tempered PlateHeavy

Alloy Steel

AISI 94B17 (Normalized & Tempered)

AISI 94B17 Normalized & Tempered PlateHeavy for engineering applications.

Chemical Composition (%)

B0.0005
C0.15
CR0.3
MN0.7
MO0.08
NI0.3
SI0.15

Mechanical Properties

Yield:400MPa; Tensile:530MPa; Elong:15%; 165HB

Chinese Standard

AISI/SAE

Applications

Shafts, gears, axles, bolts, connecting rods, crankshafts, forgings

Comments 0