A193 B16

Alloy Steel

A193 B16 / CrMoV

A193 B16 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.36
SI0.15
MN0.45
P0.035
S0.04
CR0.8
MO0.5
V0.25

Available Forms

Bar, Plate, Tube, Forging, Wire

Uses

Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.975%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.575%) raises high-temperature strength and prevents temper embrittlement. Vanadium (≈0.3%) refines grain and strengthens the tempered structure. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).