ASP30
OtherASP30
PM high speed steel with Co, improved hot hardness. PM counterpart of M30.
Chemical Composition (%)
| C | 1.2 |
|---|---|
| W | 5.8 |
| MO | 4.6 |
| CR | 3.75 |
| V | 2.7 |
| CO | 7.5 |
| P | 0.03 |
| S | 0.03 |
Mechanical Properties
Hardness(annealed):≤280 HB;Hardness(hardened):65-67 HRC
Chinese Standard
ASP30
Equivalent Grades
PM-M30 Grade
Applications
Cutting tools, broaches, hobs
Available Forms
Bar
Uses
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈8%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Heat Treatment
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Precautions
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.