ASP60

Other

ASP60

PM high speed steel, highest wear resistance of ASP series. High Co & V.

Chemical Composition (%)

C2.15
W5.8
MO6.5
CR3.75
V5.75
CO9.5
P0.03
S0.03

Mechanical Properties

Hardness(annealed):≤310 HB;Hardness(hardened):66-69 HRC

Chinese Standard

ASP60

Equivalent Grades

PM-T15 Equivalent

Applications

Heavy-duty cutting, high-speed machining

Available Forms

Bar

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈10%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.