High-Temp SteelC55
Broad-spectrum corrosion-resistant Ni-base alloy. (DIN 17200; equiv UNS N06022 / ASTM B574). Nominal values—confirm mill certificate.
Chemical Composition (%)
| CR | 20 |
|---|---|
| MO | 12.5 |
| FE | 2 |
| W | 2.5 |
Mechanical Properties
Tensile:≥760 MPa;Yield:≥355 MPa
Chinese Standard
DIN 17200 C55
Equivalent Standards
ASTM B574
Equivalent Grades
UNS N06022
Applications
广谱耐蚀镍基合金。,"Plate
Available Forms
Bar"
Uses
Heat- and creep-resistant steel for elevated-temperature service with stable strength and oxidation resistance. Used in furnace parts, exhaust manifolds, turbine components, boiler tubes and engine valves.
Heat Treatment
Normally used in the solution-annealed or precipitation-hardened condition; stabilise/age per the grade (e.g., 650–800 °C ageing). Avoid long exposure in the sigma/475 °C embrittlement ranges.
Precautions
Maintain the recommended heat-treatment envelope; prolonged time in embrittlement ranges reduces ductility. Use descaling/protective atmosphere to limit scaling.