CL50
Alloy SteelCL50
Specialty steel grade. Railway wheel steel. (TB/T 1977; equiv TB/T 1977 CL60 / 60). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.55 |
|---|---|
| SI | 0.15 |
| MN | 0.6 |
Mechanical Properties
Tensile:≥880 MPa;Yield:≥490 MPa
Chinese Standard
TB / T 1977 CL50
Equivalent Standards
TB / T 1977 CL60 / 60钢,铁路车轮钢。,Forging
Applications
High-carbon grade for rails, springs, cutting tools, wear plates and components demanding high hardness and wear resistance after heat treatment. Commonly supplied as bar, plate, sheet, tube and forging.
Available Forms
Austenitize at 760–820 °C and quench (oil/water) then temper at 150–400 °C for high hardness; spheroidize anneal (680–720 °C) improves machinability of the as-rolled bar.
Uses
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).