CPM M4
OtherCPM M4
Tool and die steel for cutting, forming, punching and molding tools. Tungsten/molybdenum (≈5.5%/4.5%) give hot hardness and red-hardness for high-speed and hot-work tools. High chromium (≈4%) provides
Chemical Composition (%)
| C | 1.42 |
|---|---|
| W | 5.5 |
| MO | 4.5 |
| CR | 4 |
| V | 4 |
Applications
Tool and die steel for cutting, forming, punching and molding tools. Tungsten/molybdenum (≈5.5%/4.5%) give hot hardness and red-hardness for high-speed and hot-
Available Forms
Bar, plate, forgings, tube
Uses
Tool and die steel for cutting, forming, punching and molding tools. Tungsten/molybdenum (≈5.5%/4.5%) give hot hardness and red-hardness for high-speed and hot-work tools. High chromium (≈4%) provides wear resistance and secondary hardening. Applied to blanks, punches, extrusion dies, shear blades, plastic-mold and cold-work tooling.
Heat Treatment
Powder/HSS: preheat 800–850 °C, austenitize 1180–1230 °C (salt or vacuum), quench, triple temper 540–570 °C to ≈64–66 HRC.
Precautions
Risk of quench cracking and distortion — use graded preheating, controlled cooling and multiple tempers. Avoid overheating the austenitizing temperature. Machine in the soft annealed condition; allow for dimensional change after heat treatment. Grind with coolant to prevent rehardening cracks.