Carpenter AerMet 490

Superalloy

Carpenter AerMet 490

Proprietary/trade-name steel grade Carpenter AerMet 490

Chemical Composition (%)

NI17
CO8
MO3
TI0.1
C0.03
P0.01
S0.01

Applications

Manufacturer proprietary steel grade (trade name) per maker specification.

Available Forms

Bar, plate, sheet, tube, forgings, strip, wire, powder

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈10.5%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.