GH4169

High-Temp Steel

GH4169

Precipitation-strengthened Ni-base superalloy. (YB/T 5231; equiv GB GH4169 / UNS N07718). Nominal values—confirm mill certificate.

Chemical Composition (%)

NI50
CR17
NB+TA4.75
MO2.8
TI0.65
AL0.2
C0.08
MN0.35
SI0.35
P0.015
S0.015
B0.006

Mechanical Properties

Tensile:≥1275 MPa;Yield:≥1035 MPa;Elong:≥12%;Hardness:≥36 HRC

Chinese Standard

T 5231 GH4169

Equivalent Standards

GB GH4169

Equivalent Grades

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.

Applications

沉淀强化镍基合金。,"Bar

Available Forms

Forging

Uses

Plate"

Heat Treatment

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Precautions

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.