Gr5
TitaniumGr5
(IS 7589). Nominal values—confirm mill certificate.
Chemical Composition (%)
| AL | 5.5 |
|---|---|
| V | 3.5 |
| FE | 0.3 |
| O | 0.2 |
Mechanical Properties
Tensile:≥895 MPa;Yield:≥828 MPa;Elong:≥10%;RA:≥25%
Equivalent Grades
IS 7589 Gr5
Available Forms
Bar,Plate
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Vanadium (≈4%) refines grain and strengthens the tempered structure. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Austenitize at 760–820 °C and quench (oil/water) then temper at 150–400 °C for high hardness; spheroidize anneal (680–720 °C) improves machinability of the as-rolled bar.
Precautions
Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).