Hastelloy C-2000 alloy

High-Temp Steel

Hastelloy C-2000 alloy

Hastelloy C-2000 alloy grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

FE3
C0.01
SI0.08
MN0.5
P0.025
S0.01
CR22
CU1.3

Available Forms

Bar, Forging, Sheet, Wire

Uses

Heat- and creep-resistant steel for elevated-temperature service with stable strength and oxidation resistance. Used in furnace parts, exhaust manifolds, turbine components, boiler tubes and engine valves.

Heat Treatment

Normally used in the solution-annealed or precipitation-hardened condition; stabilise/age per the grade (e.g., 650–800 °C ageing). Avoid long exposure in the sigma/475 °C embrittlement ranges.

Precautions

Maintain the recommended heat-treatment envelope; prolonged time in embrittlement ranges reduces ductility. Use descaling/protective atmosphere to limit scaling.