Inconel 625

High-Temp Steel

Inconel 625

Nickel-chromium superalloy with exceptional corrosion & heat resistance.

Chemical Composition (%)

NI58
CR20
MO8
NB+TA3.15
FE5
C0.1
MN0.5
SI0.5
AL0.4
TI0.4
P0.015
S0.015

Mechanical Properties

Tensile:≥830 MPa;Yield:≥415 MPa;Elong:≥30%;Hardness:≤240 HB

Chinese Standard

ASTM B446

Equivalent Grades

UNS N06625 / DIN 2.4856 / EN 2.4856

Applications

Aerospace, marine, chemical, nuclear.

Available Forms

Bar, Rod, Plate

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.

Comments 0