K465

High-Temp Steel

K465

K465 Ni-base cast superalloy. (GB/T 14992; equiv GB K465). Nominal values—confirm mill certificate.

Chemical Composition (%)

CR8.5
CO9.5
W9.5
AL5
TA3.5

Mechanical Properties

Tensile:≥690 MPa;Yield:≥280 MPa;Elong:≥25%

Chinese Standard

T 14992 K465

Equivalent Standards

GB K465

Available Forms

Cast

Uses

Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈10%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.

Heat Treatment

Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.

Precautions

Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.