Lapis
Stainless SteelLapis
Specialty steel grade. tainless steel. (AMS 5629; equiv Lapis / 13-8Mo). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.05 |
|---|---|
| CR | 12.25 |
| NI | 7.5 |
| MO | 2 |
| AL | 0.9 |
Mechanical Properties
Tensile (H1000):≥1345 MPa;Yield:≥1275 MPa;Elong:≥12%
Chinese Standard
AMS 5629 Lapis
Equivalent Standards
13-8Mo
Applications
马氏体PH,高韧高强。,Bar
Available Forms
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈8%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈2.25%) enhances resistance to chloride pitting and crevice corrosion — suited to marine and chemical service. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Uses
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Heat Treatment
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.
Precautions
Lapis
Comments 0