S355JH

Alloy Steel

S355JH

EN 10210/10219 hollow-section steel S355JH.

Chemical Composition (%)

C0.1
SI0.15
MN0.6
P0.035
S0.035

Mechanical Properties

Tensile:≥450 MPa;Yield:≥280 MPa;Elongation:≥20%

Chinese Standard

EN 10210

Equivalent Standards

EN S355JH

Applications

Structural tubing

Available Forms

Tube

Uses

Low-carbon grade used for welded structures, shafts, pins, bolts, nuts, seamless tubes and general engineering components where moderate strength and good weldability are required. Commonly supplied as bar, plate, sheet, tube and forging.

Heat Treatment

Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.

Precautions

Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).