S41020

Stainless Steel

S41020

UNS S-series stainless/heat-resisting S41020

Chemical Composition (%)

C0.15
CR11.5
P0.04
S0.03

Applications

Stainless or heat-resisting steel per ASTM/UNS.

Available Forms

Bar, plate, sheet, tube, forgings, strip, wire

Uses

Martensitic stainless steel combining moderate corrosion resistance with high strength and hardness after heat treatment. Used for cutlery, surgical instruments, turbine blades, valves, pumps, fasteners and bearings in mildly corrosive environments.

Heat Treatment

Annealing/quench from 980–1050 °C (oil or air) then temper 150–650 °C; lower temper gives higher hardness, higher temper improves toughness.

Precautions

Preheat and post-weld heat treat to avoid hydrogen cracking; soft anneal before heavy machining. Lower corrosion resistance than austenitic grades — not for strong chlorides.