SA515 Grade 70
Alloy SteelSA515 Grade 70
SA515 Grade 70 grade supplied by Shanxi Youte Steel (jlhsteel.net).
Chemical Composition (%)
| C | 0.31 |
|---|---|
| SI | 0.15 |
| MN | 1.2 |
| P | 0.025 |
| S | 0.025 |
Available Forms
Bar, Plate, Tube, Forging, Wire
Uses
Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).