SA516 Grade 70

Other

SA516 Grade 70 / SA516M Grade 485

SA516 Grade 70 grade supplied by Shanxi Youte Steel (jlhsteel.net).

Chemical Composition (%)

C0.27
SI0.15

Available Forms

Bar, Plate, Tube, Forging

Uses

Medium-carbon grade for machine parts such as gears, crankshafts, axles, connecting rods, spindles and forgings that need a balance of strength, toughness and machinability. Commonly supplied as bar, plate, sheet, tube and forging.

Heat Treatment

Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.

Precautions

Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).