SCr450
Alloy SteelSCr450
Cr quench & temper steel. (JIS G4105; equiv GB 50Cr / DIN 50Cr4). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.48 |
|---|---|
| MN | 0.7 |
| CR | 0.8 |
Mechanical Properties
Tensile:≥980 MPa;Yield:≥785 MPa
Chinese Standard
JIS G4105 SCr450
Equivalent Grades
GB 50Cr / DIN 50Cr4
Applications
铬调质钢。,"Bar
Available Forms
Forging"
Uses
Spring steel with high elastic limit and fatigue strength for coils, leaf springs, clips and suspension parts. Supplied as strip, wire and bar; shot-peened after forming for longer service life.
Heat Treatment
Austenitize 830–880 °C (oil quench) and temper at 400–520 °C; stress-relieve formed springs at 230–320 °C after coiling.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating). Shot-peen after coiling to improve fatigue life; avoid sharp bends and surface defects.