SNB16
Alloy SteelSNB16
JIS steel grade SNB16
Chemical Composition (%)
| C | 0.25 |
|---|---|
| CR | 0.5 |
| MO | 0.15 |
| P | 0.03 |
| S | 0.03 |
Applications
Japanese Industrial Standard steel grade per JIS specification.
Available Forms
Bar, plate, sheet, tube, forgings, strip, wire
Uses
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.85%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.275%) raises high-temperature strength and prevents temper embrittlement. Applied to gears, shafts, bolts, connecting rods, pressure parts and heavy forgings in automotive, energy and machinery sectors.
Heat Treatment
Austenitize at 820–870 °C (oil or water quench depending on section) and temper at 400–650 °C to the required strength/toughness balance.
Precautions
Preheat and control interpass temperature when welding; post-weld heat treatment or stress relief is recommended to avoid hard-zone cracking. Use low-hydrogen electrodes. Protect from decarburization during heating (controlled atmosphere or protective coating).