SUS317
Stainless SteelSUS317
High-Mo austenitic, enhanced corrosion resistance. (JIS G4303; equiv ASTM 317 / JIS SUS317). Nominal values—confirm mill certificate.
Chemical Composition (%)
| C | 0.08 |
|---|---|
| CR | 18 |
| NI | 11 |
| MO | 3 |
Mechanical Properties
Tensile:≥515 MPa;Yield:≥205 MPa
Chinese Standard
JIS G4303 SUS317
Equivalent Standards
ASTM 317
Equivalent Grades
JIS SUS317
Applications
高钼奥氏体,耐蚀更强。,"Plate
Available Forms
Bar"
Uses
Austenitic stainless steel with excellent corrosion resistance, formability and weldability; non-magnetic in annealed condition. High nickel (≈13%) stabilises the austenite and improves toughness and pitting resistance. Molybdenum (≈3.5%) enhances resistance to chloride pitting and crevice corrosion — suited to marine and chemical service. Used in food processing, chemical plant, architecture, heat exchangers, kitchenware and medical devices.
Heat Treatment
Solution anneal 1010–1150 °C followed by rapid water quench to retain austenite; not hardenable by heat treatment. Sensitization avoided by low carbon or stabilizers (Ti/Nb).
Precautions
Weld with low-carbon or stabilized filler (e.g., 316L, 347) to avoid sensitization; passivate after fabrication. Not hardenable, but work-hardens rapidly — use sharp tools and rigid setups. Avoid chloride contact for 304 in warm service; specify 316/317 for marine or aggressive media.
Comments 0