SUS630

Alloy Steel

SUS630

(JIS G4305). Nominal values—confirm mill certificate.

Chemical Composition (%)

C0.07
SI1
MN1
P0.04
S0.03
CR15
NI3
CU3
NB0.15

Mechanical Properties

Tensile(H900):≥1310 MPa;Yield(H900):≥1170 MPa;Elong(H900):≥10%;Hardness(H900):≥44 HRC

Chinese Standard

JIS G4305 SUS630

Available Forms

Bar,Plate

Uses

Ferritic stainless steel with good resistance to stress-corrosion cracking and oxidation, plus formability and lower cost. Used for automotive trim, exhaust systems, domestic appliances, decorative and welded structures.

Heat Treatment

Annealed at 780–850 °C and air cooled; stabilize at 600–800 °C to avoid 475 °C embrittlement; not hardenable by heat treatment.

Precautions

Avoid welding in the 475 °C embrittlement and sigma-phase ranges; use matched filler and minimize heat input. Good resistance to stress-corrosion cracking.