Sanicro70
High-Temp SteelSanicro70
Specialty steel grade. ; equiv Sanicro 70 / UNS N06600). Nominal values—confirm mill certificate.
Chemical Composition (%)
| NI | 72 |
|---|---|
| CR | 14 |
| FE | 6 |
Mechanical Properties
Tensile:≥550 MPa;Yield:≥240 MPa;Elong:≥30%
Applications
镍铬耐热抗氧化。,Tube
Available Forms
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy systems.
Uses
Solution treated 1050–1250 °C and aged (≈700–900 °C) to precipitate γ′/γ″ strengtheners; processed via vacuum induction + VAR/ESR for cleanliness.
Heat Treatment
Machining is difficult — use ceramic/PCBN tools, generous coolant and rigid setups. Keep clean (vacuum/inert melting) to avoid inclusions; avoid contamination by low-melting elements.
Precautions
UNS N06600 Sanicro70 / Sanicro 70 / UNS N06600