Sn36Pb62Ag2
TinSn36Pb62Ag2
Tin alloy (solder/bearing/pewter) Sn36Pb62Ag2.
Chemical Composition (%)
| SN | 96.5 |
|---|---|
| AG | 3 |
| CU | 0.5 |
Mechanical Properties
Liquidus:≤250 C;Solidus:≥180 C
Equivalent Grades
Tin Sn36Pb62Ag2
Applications
Soldering, bearings, coating
Available Forms
Bar,Wire,Paste
Uses
Tin-base alloy for soldering, bearings and corrosion-resistant coatings. Used in electronics soldering, babbitt bearings and pewter.
Heat Treatment
Solder alloys are used as-cast or reflowed; bearing/babbitt alloys poured onto a shell. No conventional quench/temper cycle.
Precautions
Low melting point — avoid overheating during soldering; ensure clean surfaces for good wetting.
Comments 0