Sn58Bi

Tin

Sn58Bi

Tin alloy (solder/bearing/pewter) Sn58Bi.

Chemical Composition (%)

SN96.5
AG3
CU0.5

Mechanical Properties

Liquidus:≤250 C;Solidus:≥180 C

Equivalent Grades

Tin Sn58Bi

Applications

Soldering, bearings, coating

Available Forms

Bar,Wire,Paste

Uses

Tin-base alloy for soldering, bearings and corrosion-resistant coatings. Used in electronics soldering, babbitt bearings and pewter.

Heat Treatment

Solder alloys are used as-cast or reflowed; bearing/babbitt alloys poured onto a shell. No conventional quench/temper cycle.

Precautions

Low melting point — avoid overheating during soldering; ensure clean surfaces for good wetting.

Comments 0