TB9 Annealed

Titanium

TB9 Annealed

Titanium alloy TB9 Annealed.

Chemical Composition (%)

AL5.5
V3.5
FE0.4
O0.2
C0.1
N0.05
H0.015

Mechanical Properties

Tensile:≥895 MPa;Yield:≥830 MPa;Elongation:≥10%

Equivalent Standards

ASTM TB9 Annealed

Equivalent Grades

ASTM B

Applications

Aerospace, medical, marine

Available Forms

Bar,Sheet,Forging

Uses

Titanium alloy with outstanding strength-to-weight ratio and corrosion resistance, especially in chloride environments. Used in aerospace airframes, jet engines, medical implants, marine and chemical plant.

Heat Treatment

Solution treated 900–980 °C and aged 480–600 °C (α+β grades); anneal 700–800 °C; β-annealed for creep resistance. Keep below β-transus to avoid grain growth.

Precautions

Use sharp, high-rake tooling and appropriate coolants; galling/adhesive wear can occur. Titanium reacts with hydrogen and chlorine — keep out of pickling/HCl environments.