Toolox 44

Other

Toolox 44

SSAB high-strength steel Toolox 44.

Chemical Composition (%)

C0.1
SI0.15
MN0.6
P0.035
S0.035

Mechanical Properties

Tensile:≥450 MPa;Yield:≥280 MPa;Elongation:≥20%

Equivalent Grades

SSAB / SSAB Toolox 44

Applications

Automotive, wear, armor

Available Forms

Plate

Uses

Low-carbon grade used for welded structures, shafts, pins, bolts, nuts, seamless tubes and general engineering components where moderate strength and good weldability are required. Commonly supplied as bar, plate, sheet, tube and forging.

Heat Treatment

Typically normalized (880–920 °C, air cool) or carburized (900–930 °C) for case-hardening grades, then quenched and tempered at 150–200 °C.

Precautions

Weldable with standard procedures; preheat may be needed for thick sections or higher-carbon/ alloy grades. Protect from decarburization during heating (controlled atmosphere or protective coating).