SYQ-
SYQ-P110 · alloy
SYQ-P110
Low-alloy engineering steel with enhanced hardenability and strength from alloying elements. Chromium (≈0.95%) improves hardenability, wear and corrosion resistance. Molybdenum (≈0.2%) raises high-temperature strength and prevents temper embrittlement. Ap | Q SYQ-P110
C:0.25-0.35;Cr:0.80-1.10;Mo:0.15-0.25
SYW2
SYW295 · alloy
SYW295
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
SYW3
SYW390 · alloy
SYW390
Bar, plate, sheet, tube, forgings, strip, wire, powder |
C:0.05-0.60;Si:0.10-2.50;Mn:0.30-2.50;Cr:0.00-2.00;Ni:0.00-4.50;Mo:0.00-1.00;P:≤0.040;S:≤0.040
T1
T1 · other
T1
Tool and die steel for cutting, forming, punching and molding tools. Tungsten/molybdenum (≈18%/0%) give hot hardness and red-hardness for high-speed and hot-work tools. High chromium (≈4.125%) provides wear resistance and secondary hardening. Applied to b | ASTM A600 T1
C:0.65-0.80;W:17.0-19.0;Cr:3.75-4.50;V:0.90-1.30;P:≤0.030;S:≤0.030
T10
T10 · other
T10
Wire | T 1298 T10
C:0.95-1.05;Si:0.15-0.35;Mn:0.25-0.45;Cr:1.40-1.65
T100
T100 · alloy
T100
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T105
T105 · alloy
T105
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T10A · carbon
Carbon Tool Steel Hot-Rolled Round Bar
Φ10-80mm | GB/T 1298-2008
C:0.95-1.04; Si≤0.35; Mn≤0.40; P≤0.035; S≤0.030
T10A
T10A · alloy
T10A / T00103
Bar, Plate, Tube, Forging, Wire |
C:0.95-1.04;Si:≤0.35;Mn:≤0.4;P:≤0.03;S:≤0.02;Cr:≤0.25;Ni:≤0.2;Cu:≤0.25
T11
T11 · alloy
T11
Bar,Plate | ASTM A213 T11
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T110
T110 · alloy
T110
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T115
T115 · alloy
T115
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T12
T12 · alloy
T12
Bar,Plate | ASTM A213 T12
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T120
T120 · alloy
T120
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T122
T122 · alloy
T122
Bar,Plate | ASTM A213 T122
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T13
T13 · other
T13
Wire | T 1298 T13
C:0.95-1.05;Si:0.15-0.35;Mn:0.25-0.45;Cr:1.40-1.65
T135
T135 · alloy
T135
Bar,Plate |
C:0.30-0.45;Mn:0.60-1.00;Si:0.15-0.35;Cr:0.50-1.00;P:≤0.035;S:≤0.040
T15
T15 · other
T15
Nickel/cobalt-base superalloy retaining high strength, creep and corrosion resistance at extreme temperature. Cobalt (≈5%) raises hot corrosion and wear resistance. Used in gas-turbine blades, aero-engine hot sections, combustors and advanced energy syste | ASTM A600 T15
C:1.50-1.60;W:11.0-13.0;Cr:3.75-5.00;V:4.50-5.25;Co:4.75-5.25;P:≤0.030;S:≤0.030